How is galvanic corrosion of the propeller prevented?

Galvanic corrosion arises when dissimilar metals are electrically connected in water; the anode is the part that volunteers to be consumed. Rapid anode erosion is a sign that the system is overloaded rather than working.

Why it works this way

The usual cause of overload is stray current. Replacing anodes without measuring is a dressing rather than a cure — the underlying circuit keeps consuming whatever is fitted next.

Related services

Serkan Kotel · independent yacht surveyor · IIMS · ABYC · MCA

Contact

Book your survey

Tell us where the vessel lies and your approximate date — we reply the same day.

Serkan Kotel — yacht surveyor, portrait

Serkan Kotel

Yacht surveyor · IIMS · ABYC · MCA — the person who answers the phone, walks the boat and signs the report is the same person.

Service areas

Bodrum · Yalıkavak · Turgutreis · Milas · Göcek · Fethiye · Marmaris · Datça · İstanbul · Ayvalık · Antalya

Message on WhatsApp